Recommended settings with 0.4 mm nozzle:
CURA: Special Modes -> Spiralize Outer Contour
S3D: Layer -> Single outline (Vase Mode)
Slic3r: Print setting -> Spiral vase
NO SUPPORT!
50% size ( 25 minute):
Layer height: = 0.11
Line width/Extrusion Width: 0.55*
Speed: 40 mm/sec or slower (20 mm/sec Wall)
Minimum layer time: 2s
Temperature: +5C
Fan: 75%**
100% size (80 minute):
Layer height: 0.13
Line width/Extrusion Width: 0.65*
Speed: 50 mm/sec or slower (25 mm/sec Wall)
Minimum layer time: 4s
Temperature: +10 C°
Fan: 75%**
200% size (210 minute):
Layer height: 0.17
Line width/Extrusion Width: 0.8*
Speed: 60 mm/sec or slower (30 mm/sec Wall)
Minimum layer time: 6s
Temperature: +15 C°
Fan: 75%*
Yes, it is possible to change the width of the line, up to 0.8 mm even with a nozzle from 0.4 mm
**Only for PLA and for better interlayer adhesion, but if the overhang are wrong, increased to 100 as well. (PETG 100%, ABS 0%)